- Densities of the elements (data page)
-
<< Chemical elements data references
Contents
Density, solid phase
3 Li lithium use 0.534 g/cm3 WEL (near r.t.) 535 kg/m3 LNG (at 20 °C) 0.534 g/cm3 CRC (near r.t.) 0.534 g/cm3 4 Be beryllium use 1.85 g/cm3 WEL (near r.t.) 1848 kg/m3 LNG (at 20 °C) 1.8477 g/cm3 CRC (near r.t.) 1.85 g/cm3 5 B boron use 2.34 g/cm3 WEL (near r.t.) 2460 kg/m3 LNG (at r.t.) 2.34 g/cm3 CRC (near r.t.) 2.34 g/cm3 6 C carbon (graphite) use 2.267 g/cm3 WEL (near r.t.) 2267 kg/m3 LNG (at r.t.) 2.267 g/cm3 CRC (near r.t.) 2.2 g/cm3 6 C carbon (diamond) use 3.513 g/cm3 LNG (at r.t.) 3.513 g/cm3 CRC (near r.t.) 3.513 g/cm3 11 Na sodium use 0.968 g/cm3 WEL (near r.t.) 968 kg/m3 LNG (at 20 °C) 0.968 g/cm3 CRC (near r.t.) 0.97 g/cm3 12 Mg magnesium use 1.738 g/cm3 WEL (near r.t.) 1738 kg/m3 LNG (at 20 °C) 1.738 g/cm3 CRC (near r.t.) 1.74 g/cm3 13 Al aluminium use 2.70 g/cm3 WEL (near r.t.) 2700 kg/m3 LNG (at r.t.) 2.70 g/cm3 CRC (near r.t.) 2.70 g/cm3 14 Si silicon use 2.33 g/cm3 WEL (near r.t.) 2330 kg/m3 LNG (at r.t.) 2.33 g/cm3 CRC (near r.t.) 2.3290 g/cm3 15 P phosphorus (white) use 1.823 g/cm3 WEL (near r.t.) 1823 kg/m3 LNG (at 25 °C) 1.823 g/cm3 CRC (near r.t.) 1.823 g/cm3 15 P phosphorus (red) use 2.34 g/cm3 LNG (at r.t.) 2.34 g/cm3 CRC (near r.t.) 2.16 g/cm3 15 P phosphorus (black) use 2.69 g/cm3 CRC (near r.t.) 2.69 g/cm3 16 S sulfur (orthorhombic, alpha) use 2.08 g/cm3 WEL ? (1960 kg/m3) LNG (at 20 °C) 2.08 g/cm3 CRC (near r.t.) 2.07 g/cm3 16 S sulfur (monoclinic, beta) use 1.96 g/cm3 WEL ? (1960 kg/m3) LNG (at r.t.) 1.96 g/cm3 CRC ? (near r.t.) 2.07 g/cm3 16 S sulfur (gamma) use 1.92 g/cm3 LNG (at r.t.) 1.92 g/cm3 19 K potassium use 0.89 g/cm3 WEL (near r.t.) 856 kg/m3 LNG (at r.t.) 0.89 g/cm3 CRC (near r.t.) 0.89 g/cm3 20 Ca calcium use 1.55 g/cm3 WEL (near r.t.) 1550 kg/m3 LNG (at r.t.) 1.55 g/cm3 CRC (near r.t.) 1.54 g/cm3 21 Sc scandium (hexagonal ?) use 2.985 g/cm3 WEL (near r.t.) 2985 kg/m3 LNG (at r.t.) (hexagonal) 2.985 g/cm3 CRC (near r.t.) 2.99 g/cm3 22 Ti titanium (hexagonal ?) use 4.506 g/cm3 WEL (near r.t.) 4507 kg/m3 LNG (at r.t.) (hexagonal) 4.506 g/cm3 CRC (near r.t.) 4.506 g/cm3 23 V vanadium use 6.0 g/cm3 WEL (near r.t.) 6110 kg/m3 LNG (at 19 °C) 6.11 g/cm3 CRC (near r.t.) 6.0 g/cm3 24 Cr chromium use 7.15 g/cm3 WEL (near r.t.) 7140 kg/m3 LNG (at r.t.) 7.15 g/cm3 CRC (near r.t.) 7.15 g/cm3 25 Mn manganese use 7.21 g/cm3 WEL (near r.t.) 7470 kg/m3 LNG (at 20 °C) 7.21 g/cm3 CRC (near r.t.) 7.3 g/cm3 26 Fe iron use 7.86 g/cm3 WEL (near r.t.) 7874 kg/m3 LNG (at r.t.) 7.86 g/cm3 CRC (near r.t.) 7.87 g/cm3 27 Co cobalt use 8.90 g/cm3 WEL (near r.t.) 8900 kg/m3 LNG (at r.t.) 8.90 g/cm3 CRC (near r.t.) 8.86 g/cm3 28 Ni nickel use 8.908 g/cm3 WEL (near r.t.) 8908 kg/m3 LNG (at 20 °C) 8.908 g/cm3 CRC (near r.t.) 8.90 g/cm3 29 Cu copper use 8.96 g/cm3 WEL (near r.t.) 8920 kg/m3 LNG (at 20 °C) 8.96 g/cm3 CRC (near r.t.) 8.96 g/cm3 30 Zn zinc use 7.14 g/cm3 WEL (near r.t.) 7140 kg/m3 LNG (at r.t.) 7.14 g/cm3 CRC (near r.t.) 7.14 g/cm3 31 Ga gallium use 5.91 g/cm3 WEL (near r.t.) 5904 kg/m3 LNG (at 29.6 °C) 5.904 g/cm3 CRC (near r.t.) 5.91 g/cm3 32 Ge germanium use 5.323 g/cm3 WEL (near r.t.) 5323 kg/m3 LNG (at r.t.) 5.323 g/cm3 CRC (near r.t.) 5.3234 g/cm3 33 As arsenic use 5.727 g/cm3 WEL (near r.t.) 5727 kg/m3 LNG (at 25 °C) (5.727 rel. to water at 4 °C) CRC (near r.t.) 5.75 g/cm3 34 Se selenium (hexagonal, gray) use 4.81 g/cm3 WEL (near r.t.) 4819 kg/m3 LNG (at 20 °C) (4.81 rel. to water at 4 °C) CRC (near r.t.) 4.81 g/cm3 34 Se selenium (alpha) use 4.39 g/cm3 WEL ? (4819 kg/m3) CRC (near r.t.) 4.39 g/cm3 34 Se selenium (vitreous) use 4.28 g/cm3 WEL ? (4819 kg/m3) CRC (near r.t.) 4.28 g/cm3 37 Rb rubidium use 1.532 g/cm3 WEL (near r.t.) 1532 kg/m3 LNG (at r.t.) 1.532 g/cm3 CRC (near r.t.) 1.53 g/cm3 38 Sr strontium use 2.64 g/cm3 WEL (near r.t.) 2630 kg/m3 LNG (at r.t.) 2.64 g/cm3 CRC (near r.t.) 2.64 g/cm3 39 Y yttrium use 4.472 g/cm3 WEL (near r.t.) 4472 kg/m3 LNG (at r.t.) 4.472 g/cm3 CRC (near r.t.) 4.47 g/cm3 40 Zr zirconium use 6.52 g/cm3 WEL (near r.t.) 6511 kg/m3 LNG (at r.t.) 6.52 g/cm3 CRC (near r.t.) 6.52 g/cm3 41 Nb niobium use 8.57 g/cm3 WEL (near r.t.) 8570 kg/m3 LNG (at 20 °C) 8.57 g/cm3 CRC (near r.t.) 8.57 g/cm3 42 Mo molybdenum use 10.28 g/cm3 WEL (near r.t.) 10280 kg/m3 LNG (at r.t.) 10.28 g/cm3 CRC (near r.t.) 10.2 g/cm3 43 Tc technetium (Tc-98 ?) use 11 g/cm3 WEL (near r.t.) 11500 kg/m3 LNG (at r.t.) (Tc-98) 11 g/cm3 CRC (near r.t.) 11 g/cm3 44 Ru ruthenium use 12.45 g/cm3 WEL (near r.t.) 12370 kg/m3 LNG (at 20 °C) (12.45 rel. to water at 4 °C) CRC (near r.t.) 12.1 g/cm3 45 Rh rhodium use 12.41 g/cm3 WEL (near r.t.) 12450 kg/m3 LNG (at 20 °C) 12.41 g/cm3 CRC (near r.t.) 12.4 g/cm3 46 Pd palladium use 12.023 g/cm3 WEL (near r.t.) 12023 kg/m3 LNG (at 20 °C) 12.023 g/cm3 CRC (near r.t.) 12.0 g/cm3 47 Ag silver use 10.49 g/cm3 WEL (near r.t.) 10490 kg/m3 LNG (at r.t.) 10.49 g/cm3 CRC (near r.t.) 10.5 g/cm3 48 Cd cadmium use 8.65 g/cm3 WEL (near r.t.) 8650 kg/m3 LNG (at 25 °C) 8.65 g/cm3 CRC (near r.t.) 8.69 g/cm3 49 In indium use 7.31 g/cm3 WEL (near r.t.) 7310 kg/m3 LNG (at r.t.) 7.31 g/cm3 CRC (near r.t.) 7.31 g/cm3 50 Sn tin (white) use 7.265 g/cm3 WEL (near r.t.) 7310 kg/m3 LNG (at r.t.) 7.265 g/cm3 CRC (near r.t.) 7.265 g/cm3 50 Sn tin (gray) use 5.769 g/cm3 CRC (near r.t.) 5.769 g/cm3 51 Sb antimony use 6.697 g/cm3 WEL (near r.t.) 6697 kg/m3 LNG (at 25 °C) 6.697 g/cm3 CRC (near r.t.) 6.68 g/cm3 52 Te tellurium use 6.24 g/cm3 WEL (near r.t.) 6240 kg/m3 LNG (at r.t.) 6.24 g/cm3 CRC (near r.t.) 6.24 g/cm3 53 I iodine (I2) use 4.933 g/cm3 WEL (near r.t.) 4940 kg/m3 LNG (at 25 °C) 4.63 g/cm3 CRC (near r.t.) 4.933 g/cm3 55 Cs caesium use 1.93 g/cm3 WEL (near r.t.) 1879 kg/m3 LNG (at 15 °C) 1.8785 g/cm3 CRC (near r.t.) 1.93 g/cm3 56 Ba barium use 3.51 g/cm3 WEL (near r.t.) 3510 kg/m3 LNG (at 20 °C) 3.51 g/cm3 CRC (near r.t.) 3.62 g/cm3 57 La lanthanum use 6.162 g/cm3 WEL (near r.t.) 6146 kg/m3 LNG (at r.t.) 6.162 g/cm3 CRC (near r.t.) 6.15 g/cm3 58 Ce cerium use 6.770 g/cm3 WEL (near r.t.) 6689 kg/m3 LNG (at r.t.) 6.773 g/cm3 CRC (near r.t.) 6.770 g/cm3 59 Pr praseodymium (alpha ?) use 6.77 g/cm3 WEL (near r.t.) 6640 kg/m3 LNG (at r.t.) (alpha) 6.475 g/cm3 CRC (near r.t.) 6.77 g/cm3 60 Nd neodymium use 7.01 g/cm3 WEL (near r.t.) 6800 kg/m3 LNG (at r.t.) 7.01 g/cm3 CRC (near r.t.) 7.01 g/cm3 61 Pm promethium (Pm-147 ?) use 7.26 g/cm3 WEL (near r.t.) 7264 kg/m3 LNG (at r.t.) (Pm-147) 7.22 g/cm3 CRC (near r.t.) 7.26 g/cm3 62 Sm samarium use 7.52 g/cm3 WEL (near r.t.) 7353 kg/m3 LNG (at r.t.) 7.52 g/cm3 CRC (near r.t.) 7.52 g/cm3 63 Eu europium use 5.244 g/cm3 WEL (near r.t.) 5244 kg/m3 LNG (at r.t.) 5.244 g/cm3 CRC (near r.t.) 5.24 g/cm3 64 Gd gadolinium use 7.90 g/cm3 WEL (near r.t.) 7901 kg/m3 LNG (at r.t.) 7.90 g/cm3 CRC (near r.t.) 7.90 g/cm3 65 Tb terbium use 8.23 g/cm3 WEL (near r.t.) 8219 kg/m3 LNG (at r.t.) 8.23 g/cm3 CRC (near r.t.) 8.23 g/cm3 66 Dy dysprosium use 8.540 g/cm3 WEL (near r.t.) 8551 kg/m3 LNG (at 25 °C) 8.540 g/cm3 CRC (near r.t.) 8.55 g/cm3 67 Ho holmium use 8.79 g/cm3 WEL (near r.t.) 8795 kg/m3 LNG (at r.t.) 8.79 g/cm3 CRC (near r.t.) 8.80 g/cm3 68 Er erbium use 9.066 g/cm3 WEL (near r.t.) 9066 kg/m3 LNG (at r.t.) 9.066 g/cm3 CRC (near r.t.) 9.07 g/cm3 69 Tm thulium use 9.32 g/cm3 WEL (near r.t.) 9321 kg/m3 LNG (at r.t.) 9.32 g/cm3 CRC (near r.t.) 9.32 g/cm3 70 Yb ytterbium use 6.90 g/cm3 WEL (near r.t.) 6570 kg/m3 LNG (at r.t.) 6.90 g/cm3 CRC (near r.t.) 6.90 g/cm3 71 Lu lutetium use 9.841 g/cm3 WEL (near r.t.) 9841 kg/m3 LNG (at r.t.) 9.841 g/cm3 CRC (near r.t.) 9.84 g/cm3 72 Hf hafnium use 13.31 g/cm3 WEL (near r.t.) 13310 kg/m3 LNG (at r.t.) 13.31 g/cm3 CRC (near r.t.) 13.3 g/cm3 73 Ta tantalum use 16.69 g/cm3 WEL (near r.t.) 16650 kg/m3 LNG (at r.t.) 16.69 g/cm3 CRC (near r.t.) 16.4 g/cm3 74 W tungsten use 19.25 g/cm3 WEL (near r.t.) 19250 kg/m3 LNG (at r.t.) 19.25 g/cm3 CRC (near r.t.) 19.3 g/cm3 75 Re rhenium use 21.02 g/cm3 WEL (near r.t.) 21020 kg/m3 LNG (at r.t.) 21.02 g/cm3 CRC (near r.t.) 20.8 g/cm3 76 Os osmium use 22.61 g/cm3 WEL (near r.t.) 22610 kg/m3 LNG (at 20 °C) 22.61 g/cm3 CRC (near r.t.) 22.59 g/cm3 77 Ir iridium use 22.65 g/cm3 WEL (near r.t.) 22650 kg/m3 LNG (at 20 °C) (22.65 rel. to water at 4 °C) CRC (near r.t.) 22.5 g/cm3 78 Pt platinum use 21.45 g/cm3 WEL (near r.t.) 21090 kg/m3 LNG (at 20 °C) 21.09 g/cm3 CRC (near r.t.) 21.5 g/cm3 References according to http://hypertextbook.com/facts/2004/OliviaTai.shtml:
- 21.45 g/cm3 — Zumdahl, Steven S., Zumdahl, Susan L., & Decoste, Donald J. World of Chemistry. Boston: Houghton Mifflin Company, 2002: 141.
- 21.45×103 kg/m3 — Grigoriev, Igor S. & Meilikhov, Evgenii Z. Handbook of Physical Quantities. Boca Raton: CRC Press, 1997: 116.
- 21.450 g/cm3 — Savitskii, E.M. Physical Metallurgy of Platinum Metals. New York: Pergamon Press, 1978: 31.
- (20 °C) 21.45 g/cm3 — Vines, R.F. The Platinum Metals and their Alloys. New York: The International Nickel Company, Inc., 1941: 16. — "Values ranging from 21.3 to 21.5 gm/cm³ at 20°C have been reported for the density of annealed platinum; the best value being about 21.45 gm/cm³ at 20°C."
- 21.46 g/cm3 — Rose, T. Kirke. The Precious Metals, Comprising Gold, Silver and Platinum. New York: D. Van Nostrand Company, 1909: 255. — "Pure platinum, according to G. Matthey has a density of 21.46."
79 Au gold use 19.3 g/cm3 WEL (near r.t.) 19300 kg/m3 LNG (at r.t.) 19.3 g/cm3 CRC (near r.t.) 19.3 g/cm3 81 Tl thallium use 11.85 g/cm3 WEL (near r.t.) 11850 kg/m3 LNG (at r.t.) 11.85 g/cm3 CRC (near r.t.) 11.8 g/cm3 82 Pb lead use 11.34 g/cm3 WEL (near r.t.) 11340 kg/m3 LNG (at 20 °C) (face-centered cubic) (11.34 rel. to water at 4 °C) CRC (near r.t.) 11.3 g/cm3 83 Bi bismuth use 9.78 g/cm3 WEL (near r.t.) 9780 kg/m3 LNG (at r.t.) 9.78 g/cm3 CRC (near r.t.) 9.79 g/cm3 84 Po polonium (alpha) use 9.196 g/cm3 WEL (near r.t.) 9196 kg/m3 LNG (at r.t.) 9.196 g/cm3 CRC (near r.t.) 9.20 g/cm3 84 Po polonium (beta) use 9.398 g/cm3 LNG (at r.t.) 9.398 g/cm3 85 At astatine use ? 87 Fr francium use ? 1.87 g/cm3 88 Ra radium use 5.5 g/cm3 WEL (near r.t.) 5000 kg/m3 LNG (at r.t.) 5.5 g/cm3 CRC (near r.t.) 5 g/cm3 89 Ac actinium (Ac-227 ?) use 10 g/cm3 WEL (near r.t.) 10070 kg/m3 LNG (at r.t.) (Ac-227) 10.07 g/cm3 CRC (near r.t.) 10 g/cm3 90 Th thorium use 11.7 g/cm3 WEL (near r.t.) 11724 kg/m3 LNG (at r.t.) 11.7 g/cm3 CRC (near r.t.) 11.7 g/cm3 91 Pa protactinium use 15.37 g/cm3 WEL (near r.t.) 15370 kg/m3 CRC (near r.t.) 15.4 g/cm3 92 U uranium use 19.1 g/cm3 WEL (near r.t.) 19050 kg/m3 LNG (at r.t.) 19.1 g/cm3 CRC (near r.t.) 19.1 g/cm3 93 Np neptunium use 20.2 g/cm3 WEL (near r.t.) 20450 kg/m3 LNG (at r.t.) 20.2 g/cm3 CRC (near r.t.) 20.2 g/cm3 94 Pu plutonium use 19.816 g/cm3 WEL (near r.t.) 19816 kg/m3 LNG (at 20 °C) (19.816 rel. to water at 4 °C) CRC (near r.t.) 19.7 g/cm3 95 Am americium use 12 g/cm3 LNG (at r.t.) 12 g/cm3 CRC (near r.t.) 12 g/cm3 96 Cm curium (Cm-244 ?) use 13.51 g/cm3 WEL (near r.t.) 13510 kg/m3 LNG (at r.t.) (Cm-244) 13.51 g/cm3 CRC (near r.t.) 13.51 g/cm3 97 Bk berkelium (alpha) use 14.78 g/cm3 WEL (near r.t.) 14780 kg/m3 LNG (at r.t.) 14.78 g/cm3 CRC (near r.t.) 14.78 g/cm3 97 Bk berkelium (beta) use 13.25 g/cm3 LNG (at r.t.) 13.25 g/cm3 CRC (near r.t.) 13.25 g/cm3 98 Cf californium use 15.1 g/cm3 WEL (near r.t.) 15100 kg/m3 CRC (near r.t.) 15.1 g/cm3 99 Es einsteinium use 8.84 g/cm3 LNG (at r.t.) 8.84 g/cm3 Density, liquid phase
3 Li lithium use 0.512 g/cm3 CR2 (at m.p.) 0.512 g/cm3 4 Be beryllium use 1.690 g/cm3 CR2 (at m.p.) 1.690 g/cm3 5 B boron use 2.08 g/cm3 CR2 (at m.p.) 2.08 g/cm3 11 Na sodium use 0.927 g/cm3 CR2 (at m.p.) 0.927 g/cm3 12 Mg magnesium use 1.584 g/cm3 CR2 (at m.p.) 1.584 g/cm3 13 Al aluminium use 2.375 g/cm3 CR2 (at m.p.) 2.375 g/cm3 14 Si silicon use 2.57 g/cm3 CR2 (at m.p.) 2.57 g/cm3 16 S sulfur use 1.819 g/cm3 CR2 (at m.p.) 1.819 g/cm3 17 Cl chlorine use (at -35 °C) 1.5649 g/cm3 LNG (at -35 °C) 1.5649 g/cm3 19 K potassium use 0.828 g/cm3 CR2 (at m.p.) 0.828 g/cm3 20 Ca calcium use 1.378 g/cm3 CR2 (at m.p.) 1.378 g/cm3 21 Sc scandium use 2.80 g/cm3 CR2 (at m.p.) 2.80 g/cm3 22 Ti titanium use 4.11 g/cm3 CR2 (at m.p.) 4.11 g/cm3 23 V vanadium use 5.5 g/cm3 CR2 (at m.p.) 5.5 g/cm3 24 Cr chromium use 6.3 g/cm3 CR2 (at m.p.) 6.3 g/cm3 25 Mn manganese use 5.95 g/cm3 CR2 (at m.p.) 5.95 g/cm3 26 Fe iron use 6.98 g/cm3 CR2 (at m.p.) 6.98 g/cm3 27 Co cobalt use 7.75 g/cm3 CR2 (at m.p.) 7.75 g/cm3 28 Ni nickel use 7.81 g/cm3 CR2 (at m.p.) 7.81 g/cm3 29 Cu copper use 8.02 g/cm3 CR2 (at m.p.) 8.02 g/cm3 30 Zn zinc use 6.57 g/cm3 CR2 (at m.p.) 6.57 g/cm3 31 Ga gallium use 6.095 g/cm3 LNG (at 29.8 °C, m.p. is 29.7646 °C) 6.095 g/cm3 CR2 (at m.p.) 6.08 g/cm3 32 Ge germanium use 5.60 g/cm3 CR2 (at m.p.) 5.60 g/cm3 33 As arsenic use 5.22 g/cm3 CR2 (at m.p.) 5.22 g/cm3 34 Se selenium use 3.99 g/cm3 CR2 (at m.p.) 3.99 g/cm3 35 Br bromine (Br2) use (near r.t.) 3.1028 g/cm3 LNG (at 25 °C) (3.1023 rel. to water at 4 °C) CRC (near r.t.) 3.1028 g/cm3 37 Rb rubidium use 1.46 g/cm3 CR2 (at m.p.) 1.46 g/cm3 38 Sr strontium use 6.980 g/cm3 CR2 (at m.p.) 6.980 g/cm3 39 Y yttrium use 4.24 g/cm3 CR2 (at m.p.) 4.24 g/cm3 40 Zr zirconium use 5.8 g/cm3 CR2 (at m.p.) 5.8 g/cm3 42 Mo molybdenum use 9.33 g/cm3 CR2 (at m.p.) 9.33 g/cm3 44 Ru ruthenium use 10.65 g/cm3 CR2 (at m.p.) 10.65 g/cm3 45 Rh rhodium use 10.7 g/cm3 CR2 (at m.p.) 10.7 g/cm3 46 Pd palladium use 10.38 g/cm3 CR2 (at m.p.) 10.38 g/cm3 47 Ag silver use 9.320 g/cm3 CR2 (at m.p.) 9.320 g/cm3 48 Cd cadmium use 7.996 g/cm3 CR2 (at m.p.) 7.996 g/cm3 49 In indium use 7.02 g/cm3 CR2 (at m.p.) 7.02 g/cm3 50 Sn tin use 6.99 g/cm3 CR2 (at m.p.) 6.99 g/cm3 51 Sb antimony use 6.53 g/cm3 CR2 (at m.p.) 6.53 g/cm3 52 Te tellurium use 5.70 g/cm3 CR2 (at m.p.) 5.70 g/cm3 55 Cs caesium use 1.843 g/cm3 CR2 (at m.p.) 1.843 g/cm3 56 Ba barium use 3.338 g/cm3 CR2 (at m.p.) 3.338 g/cm3 57 La lanthanum use 5.94 g/cm3 CR2 (at m.p.) 5.94 g/cm3 58 Ce cerium use 6.55 g/cm3 CR2 (at m.p.) 6.55 g/cm3 59 Pr praseodymium use 6.50 g/cm3 CR2 (at m.p.) 6.50 g/cm3 60 Nd neodymium use 6.89 g/cm3 CR2 (at m.p.) 6.89 g/cm3 62 Sm samarium use 7.16 g/cm3 CR2 (at m.p.) 7.16 g/cm3 63 Eu europium use 5.13 g/cm3 CR2 (at m.p.) 5.13 g/cm3 64 Gd gadolinium use 7.4 g/cm3 CR2 (at m.p.) 7.4 g/cm3 65 Tb terbium use 7.65 g/cm3 CR2 (at m.p.) 7.65 g/cm3 66 Dy dysprosium use 8.37 g/cm3 CR2 (at m.p.) 8.37 g/cm3 67 Ho holmium use 8.34 g/cm3 CR2 (at m.p.) 8.34 g/cm3 68 Er erbium use 8.86 g/cm3 CR2 (at m.p.) 8.86 g/cm3 69 Tm thulium use 8.56 g/cm3 CR2 (at m.p.) 8.56 g/cm3 70 Yb ytterbium use 6.21 g/cm3 CR2 (at m.p.) 6.21 g/cm3 71 Lu lutetium use 9.3 g/cm3 CR2 (at m.p.) 9.3 g/cm3 72 Hf hafnium use 12 g/cm3 CR2 (at m.p.) 12 g/cm3 73 Ta tantalum use 15 g/cm3 CR2 (at m.p.) 15 g/cm3 74 W tungsten use 17.6 g/cm3 CR2 (at m.p.) 17.6 g/cm3 75 Re rhenium use 18.9 g/cm3 CR2 (at m.p.) 18.9 g/cm3 76 Os osmium use 20 g/cm3 CR2 (at m.p.) 20 g/cm3 77 Ir iridium use 19 g/cm3 CR2 (at m.p.) 19 g/cm3 78 Pt platinum use 19.77 g/cm3 CR2 (at m.p.) 19.77 g/cm3 79 Au gold use 17.31 g/cm3 CR2 (at m.p.) 17.31 g/cm3 80 Hg mercury use (at r.t.) 13.534 g/cm3 LNG (at r.t.) 13.534 g/cm3 CRC (near r.t.) 13.5336 g/cm3 81 Tl thallium use 11.22 g/cm3 CR2 (at m.p.) 11.22 g/cm3 82 Pb lead use 10.66 g/cm3 CR2 (at m.p.) 10.66 g/cm3 83 Bi bismuth use 10.05 g/cm3 CR2 (at m.p.) 10.05 g/cm3 92 U uranium use 17.3 g/cm3 CR2 (at m.p.) 17.3 g/cm3 94 Pu plutonium use 16.63 g/cm3 CR2 (at m.p.) 16.63 g/cm3 Density, gas phase
value conditions 1 H hydrogen (H2) use 0.08988 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 0.082 g/L 25 °C, 101.325 kPa KCH 0.08988 kg/m3 0 °C, 101.3 kPa VDW 0.08988 g/L 0 °C, 101.325 kPa (lit. source) 0.08988 g/L 2 He helium use 0.1786 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 0.164 g/L 25 °C, 101.325 kPa LNG 0.176 g/L room temperature KCH 0.1785 kg/m3 0 °C, 101.3 kPa VDW 0.1786 g/L 0 °C, 101.325 kPa (lit. source) 0.1785 g/L 0°C, 1 atm 7 N nitrogen (N2) use 1.251 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 1.145 g/L 25 °C, 101.325 kPa LNG 1.165 g/L 20 °C KCH 1.2505 kg/m3 0 °C, 101.3 kPa VDW 1.251 g/L 0 °C, 101.325 kPa (lit. source) 1.2506 g/L 8 O oxygen (O2) use 1.429 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 1.308 g/L 25 °C, 101.325 kPa LNG 1.331 g/L 20 °C KCH 1.42895 kg/m3 0 °C, 101.3 kPa VDW 1.429 g/L 0 °C, 101.325 kPa (lit. source) 1.429 g/L 0 °C 9 F fluorine (F2) use 1.7 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 1.553 g/L 25 °C, 101.325 kPa VDW (lit. source) 1.696 g/L [1] 1.59 kg/m3 15 °C, 1.013 bar [2] 0.0983 lb/ft3 70 °F, 1 atm 10 Ne neon use 0.9002 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 0.825 g/L 25 °C, 101.325 kPa LNG 0.8999 g/L 0 °C KCH 0.9002 kg/m3 0 °C, 101.3 kPa VDW 0.9002 g/L 0 °C, 101.325 kPa (lit. source) 0.89990 g/L 0°C, 1 atm 17 Cl chlorine (Cl2) use 3.2 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 2.898 g/L 25 °C, 101.325 kPa LNG 2.98 g/L 20 °C KCH 3.214 kg/m3 0 °C, 101.3 kPa VDW 3.116 g/L 0 °C, 101.325 kPa (lit. source) 3.214 g/L 18 Ar argon use 1.784 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 1.633 g/L 25 °C, 101.325 kPa LNG 1.7824 g/L 0 °C KCH 1.784 kg/m3 0 °C, 101.3 kPa VDW 1.784 g/L 0 °C, 101.325 kPa (lit. source) 1.7837 g/L 36 Kr krypton use 3.749 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 3.425 g/L 25 °C, 101.325 kPa LNG 3.7493 g/L room temperature KCH 3.744 kg/m3 0 °C, 101.3 kPa VDW 3.749 g/L 0 °C, 101.325 kPa (lit. source) 3.733 g/L 0 °C 54 Xe xenon use 5.894 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 5.366 g/L 25 °C, 101.325 kPa LNG 5.761 g/L room temperature KCH 5.897 kg/m3 0 °C, 101.3 kPa VDW 5.894 g/L 0 °C, 101.325 kPa (lit. source) 5.88 g/L 86 Rn radon (Radon-222 ?) use 9.73 g/L 0 °C, 101.325 kPa CRC (calc. ideal gas) 9.074 g/L 25 °C, 101.325 kPa LNG 9.73 g/L room temperature VDW (lit. source) 9.73 g/L ICT.a 9.73 g/L 0 °C, 1 An (=101.325 kPa)
formula weight = 222Notes
- The suggested values for solid densities refer to "near room temperature" by default.
- The suggested values for liquid densities refer to "at the melting point" by default.
References
WEL
As quoted at http://www.webelements.com/ from these sources:
- A.M. James and M.P. Lord in Macmillan's Chemical and Physical Data, Macmillan, London, UK, 1992.
- D.R. Lide, (ed.) in Chemical Rubber Company handbook of chemistry and physics, CRC Press, Boca Raton, Florida, USA, 77th edition, 1996.
- J.A. Dean (ed) in Lange's Handbook of Chemistry, McGraw-Hill, New York, USA, 14th edition, 1992.
- G.W.C. Kaye and T.H. Laby in Tables of physical and chemical constants, Longman, London, UK, 15th edition, 1993.
CRC
As quoted from various sources in an online version of:
- David R. Lide (ed), CRC Handbook of Chemistry and Physics, 84th Edition. CRC Press. Boca Raton, Florida, 2003; Section 4, Properties of the Elements and Inorganic Compounds; Physical Constants of Inorganic Compounds
CR2
- David R. Lide (ed), CRC Handbook of Chemistry and Physics, 84th Edition. CRC Press. Boca Raton, Florida, 2003; Section 4, Properties of the Elements and Inorganic Compounds; Density of Molten Elements and Representative Salts
LNG
As quoted from an online version of:
- J.A. Dean (ed), Lange's Handbook of Chemistry (15th Edition), McGraw-Hill, 1999; Section 3; Table 3.2 Physical Constants of Inorganic Compounds
VDW
The following molar volumes and densities for the majority of the gaseous elements were calculated from the van der Waals equation of state, using the quoted values of the van der Waals constants. The source for the van der Waals constants and for the literature densities was: R. C. Weast (Ed.), Handbook of Chemistry and Physics (53rd Edn.), Cleveland:Chemical Rubber Co., 1972.
van der Waals constants 25°C, 100.0 kPa 0°C, 1 atm Lit. a (L2bar/mol2) b (L/mol) Vm (L) d (g/L) Vm (L) d (g/L) d (g/L) Argon 1.363 0.03219 24.77 1.613 22.39 1.784 1.7837 Chlorine 6.579 0.05622 25.11 2.824 22.75 3.116 3.214 Fluorine not available 1.696 Helium 0.03457 0.02370 24.81 0.1613 22.44 0.1786 0.1785 (0°C, 1 atm) Hydrogen 0.2476 0.02661 24.81 0.08127 22.43 0.08988 0.08988 Krypton 2.349 0.03978 24.73 3.388 22.35 3.749 3.733 (0°C) Neon 0.2135 0.01709 24.80 0.8139 22.42 0.9002 0.89990 (0°C, 1 atm) Nitrogen 1.408 0.03913 24.77 1.131 22.39 1.251 1.2506 Oxygen 1.378 0.03183 24.77 1.292 22.39 1.429 1.429 (0°C) Radon not available 9.73 Xenon 4.250 0.05105 24.69 5.323 22.28 5.894 5.88 other
- KCH: Kuchling, Horst, Taschenbuch der Physik, 13. Auflage, Verlag Harri Deutsch, Thun und Frankfurt/Main, German edition, 1991. ISBN 3-8171-1020-0
- ICT: Washburn, E.W. (ed.), International Critical Tables of Numerical Data, Physics, Chemistry and Technology (1926–1930; 2003 Knovel online version)
- (a) Gray and Ramsay, Proceedings of the Royal Society (London). A. Mathematical and Physical Sciences. 84: 536; (1911)
Categories:- Properties of chemical elements